MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient OnFlex™ U 5370A-E0077 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™ U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™ U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of both raw materials, for example the good processability and soft haptic of a TPE-S with the excellent mechanical properties and abrasion resistance of a TPE-U. OnFlex™ U 5300 compounds are formulated to deliver very good scratch resistance, a wide hardness range and good chemical resistance.

Properties are measured using injection molded plaques.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ISO 868
Tensile Strength at Break  17.7 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
2570 psi
@Thickness 0.0787 in,
Temperature 73.4 °F
Type 2, 200 mm/min Across Flow; ISO 37
 17.7 MPa
@Thickness 2.00 mm,
Temperature 23.0 °C
2570 psi
@Thickness 0.0787 in,
Temperature 73.4 °F
Type 2, 200 mm/min; Flow; ISO 37
Elongation at Break  570 %
@Thickness 2.00 mm,
Temperature 23.0 °C
570 %
@Thickness 0.0787 in,
Temperature 73.4 °F
Type 2, 200 mm/min Across Flow; ISO 37
 580 %
@Thickness 2.00 mm,
Temperature 23.0 °C
580 %
@Thickness 0.0787 in,
Temperature 73.4 °F
Type 2, 200 mm/min; Flow; ISO 37
Tear Strength  47.0 kN/m
@Thickness 2.00 mm,
Temperature 23.0 °C
268 pli
@Thickness 0.0787 in,
Temperature 73.4 °F
Method A, Trouser, 500 mm/min Across Flow; ISO 34-1
 53.0 kN/m
@Thickness 2.00 mm,
Temperature 23.0 °C
302 pli
@Thickness 0.0787 in,
Temperature 73.4 °F
Method A, Trouser, 500 mm/min; Flow; ISO 34-1
Abrasion 3535[mm³]; DIN 53516
 
Optical PropertiesMetricEnglishComments
Gloss 6.0 %6.0 %60°; ISO 2813
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 - 210 °C338 - 410 °F
Mold Temperature 30.0 - 60.0 °C86.0 - 140 °F
Drying Temperature 100 °C212 °F
Dry Time 2.00 hour2.00 hour
 
Descriptive Properties
AppearanceMatte Finish
FeaturesGood Abrasion Resistance
 Oil Resistant
 Scratch Resistant
Fogging1.1 mgDIN 75201B; 100°C
FormsPellets
Generic MaterialTPE
Generic Material TypeThermoplastic Polyurethane Elastomer (TPU)
Generic NameThermoplastic Elastomer (TPE)
Injection RateSlow
Odor rating2.1VDA 270
Processing MethodCalendering
 Film Extrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAutomotive Applications
 Consumer Applications
 General Purpose
 Industrial Applications
 Power/Other Tools

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient OnFlex™ U 5470A-E0083 Thermoplastic Elastomer (TPE)
Covestro Texin® DP7-1157 Thermoplastic Polyurethane + ABS Blend
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy
Avient OnFlex™ U 5380A-S0013 Thermoplastic Elastomer (TPE)
API Megol AM DP2268/65PA12 SEBS Adhesion Modified Overmolding for PA

PH0POL1001 / 145570

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.