Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.23 g/cc | 1.23 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 75 | 75 |
| 60 @Treatment Temp. 23.0 °C, Time 252000 sec | 60 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 64 @Treatment Temp. 23.0 °C, Time 252000 sec | 64 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 70 @Treatment Temp. 150 °C, Time 252000 sec | 70 @Treatment Temp. 302 °F, Time 70.0 hour |
| 72 @Treatment Temp. 100 °C, Time 252000 sec | 72 @Treatment Temp. 212 °F, Time 70.0 hour |
| 72 @Treatment Temp. 125 °C, Time 252000 sec | 72 @Treatment Temp. 257 °F, Time 70.0 hour |
| 73 @Treatment Temp. 100 °C, Time 252000 sec | 73 @Treatment Temp. 212 °F, Time 70.0 hour |
| 74 @Treatment Temp. 23.0 °C, Time 252000 sec | 74 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 75 @Treatment Temp. 100 °C, Time 252000 sec | 75 @Treatment Temp. 212 °F, Time 70.0 hour |
| 75 @Treatment Temp. 125 °C, Time 252000 sec | 75 @Treatment Temp. 257 °F, Time 70.0 hour |
| 75 @Treatment Temp. 150 °C, Time 252000 sec | 75 @Treatment Temp. 302 °F, Time 70.0 hour |
| 77 @Treatment Temp. 100 °C, Time 252000 sec | 77 @Treatment Temp. 212 °F, Time 70.0 hour |
| 77 @Treatment Temp. 100 °C, Time 252000 sec | 77 @Treatment Temp. 212 °F, Time 70.0 hour |
| 80 @Treatment Temp. 125 °C, Time 252000 sec | 80 @Treatment Temp. 257 °F, Time 70.0 hour |
| 80 @Treatment Temp. 125 °C, Time 252000 sec | 80 @Treatment Temp. 257 °F, Time 70.0 hour |
| 81 @Treatment Temp. 150 °C, Time 252000 sec | 81 @Treatment Temp. 302 °F, Time 70.0 hour |
Tensile Strength | 23.32 MPa | 3382 psi |
| 8.6509 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 1254.7 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 12.289 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 1782.3 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 16.416 MPa @Treatment Temp. 150 °C, Time 252000 sec | 2380.9 psi @Treatment Temp. 302 °F, Time 70.0 hour |
| 21.406 MPa @Treatment Temp. 125 °C, Time 252000 sec | 3104.7 psi @Treatment Temp. 257 °F, Time 70.0 hour |
| 21.569 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 3128.3 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 22.735 MPa @Treatment Temp. 100 °C, Time 252000 sec | 3297.4 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 22.782 MPa @Treatment Temp. 125 °C, Time 252000 sec | 3304.2 psi @Treatment Temp. 257 °F, Time 70.0 hour |
| 22.782 MPa @Treatment Temp. 125 °C, Time 252000 sec | 3304.2 psi @Treatment Temp. 257 °F, Time 70.0 hour |
| 23.2015 MPa @Treatment Temp. 150 °C, Time 252000 sec | 3365.09 psi @Treatment Temp. 302 °F, Time 70.0 hour |
| 24.671 MPa @Treatment Temp. 100 °C, Time 252000 sec | 3578.2 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 24.671 MPa @Treatment Temp. 100 °C, Time 252000 sec | 3578.2 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 24.880 MPa @Treatment Temp. 125 °C, Time 252000 sec | 3608.6 psi @Treatment Temp. 257 °F, Time 70.0 hour |
| 25.300 MPa @Treatment Temp. 100 °C, Time 252000 sec | 3669.5 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 25.603 MPa @Treatment Temp. 150 °C, Time 252000 sec | 3713.4 psi @Treatment Temp. 302 °F, Time 70.0 hour |
Elongation, Ultimate | 539 % | 539 % |
| 233.9 % @Treatment Temp. 23.0 °C, Time 252000 sec | 233.9 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 246.9 % @Treatment Temp. 23.0 °C, Time 252000 sec | 246.9 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 299.1 % @Treatment Temp. 150 °C, Time 252000 sec | 299.1 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 314.8 % @Treatment Temp. 125 °C, Time 252000 sec | 314.8 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 352 % @Treatment Temp. 23.0 °C, Time 252000 sec | 352 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 362.2 % @Treatment Temp. 100 °C, Time 252000 sec | 362.2 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 383.8 % @Treatment Temp. 125 °C, Time 252000 sec | 383.8 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 390.2 % @Treatment Temp. 100 °C, Time 252000 sec | 390.2 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 396.2 % @Treatment Temp. 150 °C, Time 252000 sec | 396.2 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 523.9 % @Treatment Temp. 125 °C, Time 252000 sec | 523.9 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 523.9 % @Treatment Temp. 125 °C, Time 252000 sec | 523.9 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 561.1 % @Treatment Temp. 150 °C, Time 252000 sec | 561.1 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 574 % @Treatment Temp. 100 °C, Time 252000 sec | 574 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 574.03 % @Treatment Temp. 100 °C, Time 252000 sec | 574.03 % @Treatment Temp. 212 °F, Time 70.0 hour |
100% Modulus | 3.64 MPa | 528 psi |
Tear Strength | 36.5 kN/m | 208 pli |
| 45.1 kN/m | 257 pli |
Compression Set | 10 % @Treatment Temp. 125 °C, Time 79200 sec | 10 % @Treatment Temp. 257 °F, Time 22.0 hour |
| 10.9 % @Treatment Temp. 100 °C, Time 79200 sec | 10.9 % @Treatment Temp. 212 °F, Time 22.0 hour |
| 12.4 % @Treatment Temp. 125 °C, Time 79200 sec | 12.4 % @Treatment Temp. 257 °F, Time 22.0 hour |
| 13.2 % @Treatment Temp. 100 °C, Time 252000 sec | 13.2 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 13.4 % @Treatment Temp. 150 °C, Time 79200 sec | 13.4 % @Treatment Temp. 302 °F, Time 22.0 hour |
| 14.5 % @Treatment Temp. 100 °C, Time 252000 sec | 14.5 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 15.1 % @Treatment Temp. 100 °C, Time 79200 sec | 15.1 % @Treatment Temp. 212 °F, Time 22.0 hour |
| 17.4 % @Treatment Temp. 150 °C, Time 79200 sec | 17.4 % @Treatment Temp. 302 °F, Time 22.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | -62.2 °C | -80.0 °F |
Shrinkage | -2.60 % @Treatment Temp. 150 °C, Time 252000 sec | -2.60 % @Treatment Temp. 302 °F, Time 70.0 hour |
| -2.50 % @Treatment Temp. 125 °C, Time 252000 sec | -2.50 % @Treatment Temp. 257 °F, Time 70.0 hour |
| -2.00 % @Treatment Temp. 100 °C, Time 252000 sec | -2.00 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 0.80 % @Treatment Temp. 100 °C, Time 252000 sec | 0.80 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 3.0 % @Treatment Temp. 23.0 °C, Time 252000 sec | 3.0 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 8.6 % @Treatment Temp. 100 °C, Time 252000 sec | 8.6 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 12 % @Treatment Temp. 150 °C, Time 252000 sec | 12 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 12.8 % @Treatment Temp. 125 °C, Time 252000 sec | 12.8 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 34.5 % @Treatment Temp. 23.0 °C, Time 252000 sec | 34.5 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 56.3 % @Treatment Temp. 23.0 °C, Time 252000 sec | 56.3 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |