MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Henkel Loctite® ECCOBOND FP4451TD Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Black

Cure: Heat Cure

Product Benefits:

  • High purity
  • Excellent chemical resistance
  • Exceptional thermal stability
Application: Encapsulant - dam

Filler Type Silica

Typical Package Application: BGA and IC memory cards

LOCTITE ECCOBOND FP4451TD damming material is designed as a flow control barrier around areas of bare chip encapsulation.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.79 g/cc1.79 g/cc
Filler Content 73 %73 %
Particle Size 20 µm20 µmmedian
 <= 200 µm<= 200 µmmaximum
Brookfield Viscosity 300000 cP300000 cPSpindle 7, speed 20 rpm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.0 µm/m-°C
@Temperature 40.0 - 120 °C
11.7 µin/in-°F
@Temperature 104 - 248 °F
Cured, Below Tg
 65.0 µm/m-°C
@Temperature 190 - 220 °C
36.1 µin/in-°F
@Temperature 374 - 428 °F
Cured, Above Tg
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
Glass Transition Temp, Tg 150 °C302 °FCured, by TMA
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 125 °C
0.500 hour
@Temperature 257 °F
plus 90 minutes @ 165°C
Gel Time 13.0 min
@Temperature 121 °C
13.0 min
@Temperature 250 °F
 
Descriptive Properties
Extractable Ionic Content (ppm)<1Cured, Sodium (Na+)
 <1Cured, Potassium (K+)
 <10Cured, Chloride (Cl-)
Pot Life10 daystime to double viscosity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOCT5079 / 255290

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.