MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Super high and Very High Impact Sheeting grades for Automobile & Luggage Applications

Information provided by Bhansali

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.045 g/cc0.03775 lb/in³ASTM D-792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D-955
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106106ASTM D-785
Tensile Strength, Yield 39.2 MPa
@Thickness 3.20 mm
5690 psi
@Thickness 0.126 in
Type 1, 5 mm/min speed; ASTM D-638
Flexural Yield Strength 55.9 MPa
@Thickness 6.40 mm
8110 psi
@Thickness 0.252 in
ASTM D-790
Flexural Modulus 1.91 GPa
@Thickness 6.40 mm
277 ksi
@Thickness 0.252 in
ASTM D-790
Izod Impact, Notched  3.5294 J/cm
@Thickness 6.40 mm
6.6120 ft-lb/in
@Thickness 0.252 in
ASTM D-256
 4.5098 J/cm
@Thickness 3.20 mm
8.4487 ft-lb/in
@Thickness 0.126 in
ASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C198 °FMethod A - Annealed; ASTM D-648
Vicat Softening Point 104 °C219 °FMethod B; ASTM D-1525
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
UL-94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cossa Polimeri ESTADIENE 2506 Acrylonitrile Butadiene Styrene
Mocom (ALBIS) ALCOLOR® Function ABS UV CX BG1049-05 ABS
Mocom (ALBIS) ALCOLOR® ABS A GN76-4123 ABS
Covestro Bayblend® FR 3030 Polycarbonate + ABS, Flame Retardant Grade
Chi Mei Polylac® PA-747R ABS - Extrusion

PBHANS36 / 27145

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.