MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Super high and Very High Impact Sheeting grades for Automobile & Luggage Applications

Information provided by Bhansali

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.045 g/ccASTM D-792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmASTM D-955
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 106ASTM D-785
Tensile Strength, Yield 5690 psi
@Thickness 3.20 mm
Type 1, 5 mm/min speed; ASTM D-638
Flexural Yield Strength 8110 psi
@Thickness 6.40 mm
ASTM D-790
Flexural Modulus 277000 psi
@Thickness 6.40 mm
ASTM D-790
Izod Impact, Notched 352.94 J/m
@Thickness 6.40 mm
ASTM D-256
 450.98 J/m
@Thickness 3.20 mm
ASTM D-256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °CMethod A - Annealed; ASTM D-648
Vicat Softening Point 104 °CMethod B; ASTM D-1525
Flammability, UL94 HB
@Thickness 3.20 mm
UL-94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cossa Polimeri ESTADIENE 2506 Acrylonitrile Butadiene Styrene
Mocom (ALBIS) ALCOLOR® Function ABS UV CX BG1049-05 ABS
Mocom (ALBIS) ALCOLOR® ABS A GN76-4123 ABS
Covestro Bayblend® FR 3030 Polycarbonate + ABS, Flame Retardant Grade
Chi Mei Polylac® PA-747R ABS - Extrusion

PBHANS36 / 27145

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.