MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EN SPH235 High Manganese Pressure Vessel Carbon Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel; Pressure Vessel Steel

Key Words: EN 10207(91) SPH235. Similar to AISI 1513, UNS G15130
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/ccEstimated by MatWeb from similar grade
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 360 - 480 MPa
@Thickness 3.00 - 16.0 mm
 360 - 480 MPa
@Thickness 16.0 - 40.0 mm
 360 - 480 MPa
@Thickness 40.0 - 60.0 mm
Tensile Strength, Yield 215 MPa
@Thickness 40.0 - 60.0 mm
 225 MPa
@Thickness 16.0 - 40.0 mm
 235 MPa
@Thickness 3.00 - 16.0 mm
Elongation at Break 25 %
@Thickness 40.0 - 60.0 mm
 26 %
@Thickness 3.00 - 16.0 mm
 26 %
@Thickness 16.0 - 40.0 mm
Modulus of Elasticity 200 GPaEstimated by MatWeb from similar grade
Poissons Ratio 0.29Estimated by MatWeb from similar grade
Shear Modulus 80.0 GPaEstimated by MatWeb from similar grade
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000170 ohm-cmEstimated by MatWeb from similar grade
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°CEstimated by MatWeb from similar grade
Specific Heat Capacity 0.470 J/g-°CEstimated by MatWeb from similar grade
Thermal Conductivity 52.0 W/m-KEstimated by MatWeb from similar grade
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al >= 0.020 %
Carbon, C <= 0.16 %
Iron, Fe 98.6 - 99.6 %As Balance
Manganese, Mn 0.40 - 1.2 %
Phosphorus, P <= 0.035 %
Silicon, Si <= 0.35 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® 690 UNS N06690 Nickel Superalloy (1825°F anneal)
Special Metals Nickel 200
EN 1.0112 High Manganese Pressure Vessel Carbon Steel
EN 1.1100 High Manganese Pressure Vessel Carbon Steel
EN SPHL275 High Manganese Pressure Vessel Carbon Steel

M9ZESPH235 / 232259

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.