MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Cookson Group STAYSTIK® 501 Silver Filled Electrically Conductive Film  (discontinued **)
Categories: Polymer; Adhesive; Film; Thermoplastic

Material Notes: These thermoplastic adhesive films are designed for use in a variety of electronic applications. These materials are ideal for applications where resistance to high temperature excursions is desired. These film adhesives can be used for die attach in solder sealed, hermetic packages and have demonstrated low RGA moisture readings. This high temperature, reworkable thermoplastic system offers many unique advantages in applications traditionally ill-suited to thermoset adhesives.

Features:

  • Fully polymerized resin - No "cure"
  • Easily reworkable - No outgassing
  • Bonds in seconds - Not hours or minutes
  • Low modulus reduces stress to bonded materials

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity >= 360 ksi
Adhesive Bond Strength >= 3500 psiDie shear adhesion, at 25°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.00050 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity >= 3.00 W/m-K
Maximum Service Temperature, Air 200 °CContinuous use
 <= 400 °CExcursion Temperature
Minimum Service Temperature, Air -65.0 °CContinuous use
Glass Transition Temp, Tg 180 - 185 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Monthat 25°C
 
Descriptive Properties
Attach Temperature300-375°C
Filler MaterialSilver

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cotronics Duralco™ 120 500°F Silver Filled Epoxy, Electrically Conductive
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy
Epoxy Technology EPO-TEK® H20-HC Electrically Conductive Epoxy
Epoxy Technology EPO-TEK® 431 Copper Filled Epoxy
Dielectric Polymers NT-590DL Protective Film

PPLASK062 / 56352

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.