MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lucite International Colacryl® P2601 Specialty Polystyrene Resin
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Cross-linked polystyrene resins have much higher thermal stability than conventional thermoplastic acrylic resins. Colacryl® P2601 is stable up to around 300°C.

Suggested Uses:
This product is usually used as a filler for investment casting waxes. The product may also be used as a texturing agent for surface coatings for use in flammable atmospheres.

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 35 µm
Ash <= 0.050 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucite International Lucite® 30B Acrylic Bead Resin
Lucite International Elvacite® 4067 Acrylic Resin
Lucite International Lucite® 6751 Acrylic Bead Resin
Lucite International Colacryl® P2608 Specialty Polystyrene Resin
Lucite International Elvacite® 2044 Acrylic Resin

PLUCIT9431 / 150145

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.