MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lucite International Elvacite® 4067 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Elvacite® 4067 is a solid acrylic bead resin that has been designed to give good solubility in white spirit for use in combinations with alkyd resins.

Elvacite® 4067 has good compatibility with a wide range of short, medium and long oil alkyds and can be used to shorten drying time of alkyd-based coatings. Elvacite® 4067 may also improve color and color stability, and enhance weatherability.

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 0.20 - 0.250.20 - 0.25Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 57000 g/mol57000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.000.00
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 46.0 °C115 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.50 %0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucite International Colacryl® P2601 Specialty Polystyrene Resin
Lucite International Lucite® 6751 Acrylic Bead Resin
Lucite International Lucite® 30B Acrylic Bead Resin

PLUCIT9481 / 150195

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.