Product Description: Pentalyn™ 770-M resin is a phenolic modified rosin ester, which offers high viscosity and low solubility in mineral oils. Pentalyn™ 770-M resin also offers good gelling and is ideal for lithographic printing or offset inks in Quick-Set systems or as modifying resin Heat-Set and Flushing, designed for modern high-speed printing equipment. Application/Uses: - Graphic Arts
- Hot Melt Adhesives
- Solventborne Adhesives
Key Attributes:- Good gelling
- High viscosity
- Low solubility in mineral oils
Information provided by Eastman |