MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Pentalyn™ 770-M Resin
Categories: Polymer

Material Notes: Product Description: Pentalyn™ 770-M resin is a phenolic modified rosin ester, which offers high viscosity and low solubility in mineral oils. Pentalyn™ 770-M resin also offers good gelling and is ideal for lithographic printing or offset inks in Quick-Set systems or as modifying resin Heat-Set and Flushing, designed for modern high-speed printing equipment.

Application/Uses:

  • Graphic Arts
  • Hot Melt Adhesives
  • Solventborne Adhesives
Key Attributes:
  • Good gelling
  • High viscosity
  • Low solubility in mineral oils

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 2020[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 159 °C318 °FASTM E28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 10<= 10
 
Descriptive Properties
AppearanceCrystalline Solid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5494 / 222688

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.