MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik SANMAC 4541 Billet
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: Sanmac 4541, is a titanium stabilized austenitic chrome-nickel steel with improved machinability.

Information provided by Sandvik

ASTM 321; UNS S32100; EN 1.4541

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 215<= 215
Tensile Strength, Ultimate 515 - 700 MPa74700 - 102000 psi
 >= 360 MPa
@Temperature 500 °C
>= 52200 psi
@Temperature 932 °F
 >= 375 MPa
@Temperature 300 °C
>= 54400 psi
@Temperature 572 °F
 >= 375 MPa
@Temperature 400 °C
>= 54400 psi
@Temperature 752 °F
 >= 390 MPa
@Temperature 200 °C
>= 56600 psi
@Temperature 392 °F
 >= 440 MPa
@Temperature 100 °C
>= 63800 psi
@Temperature 212 °F
Tensile Strength, Yield  >= 210 MPa
@Strain 0.2 %
>= 30500 psi
@Strain 0.2 %
 >= 245 MPa
@Strain 1 %
>= 35500 psi
@Strain 1 %
 >= 119 MPa
@Strain 0.2 %,
Temperature 500 °C
>= 17300 psi
@Strain 0.2 %,
Temperature 932 °F
 >= 125 MPa
@Strain 0.2 %,
Temperature 400 °C
>= 18100 psi
@Strain 0.2 %,
Temperature 752 °F
 >= 135 MPa
@Strain 0.2 %,
Temperature 300 °C
>= 19600 psi
@Strain 0.2 %,
Temperature 572 °F
 >= 149 MPa
@Strain 1 %,
Temperature 500 °C
>= 21600 psi
@Strain 1 %,
Temperature 932 °F
 >= 155 MPa
@Strain 0.2 %,
Temperature 200 °C
>= 22500 psi
@Strain 0.2 %,
Temperature 392 °F
 >= 156 MPa
@Strain 1 %,
Temperature 400 °C
>= 22600 psi
@Strain 1 %,
Temperature 752 °F
 >= 167 MPa
@Strain 1 %,
Temperature 300 °C
>= 24200 psi
@Strain 1 %,
Temperature 572 °F
 >= 175 MPa
@Strain 0.2 %,
Temperature 100 °C
>= 25400 psi
@Strain 0.2 %,
Temperature 212 °F
 >= 185 MPa
@Strain 1 %,
Temperature 200 °C
>= 26800 psi
@Strain 1 %,
Temperature 392 °F
 >= 205 MPa
@Strain 1 %,
Temperature 100 °C
>= 29700 psi
@Strain 1 %,
Temperature 212 °F
Elongation at Break >= 40 %>= 40 %
Reduction of Area >= 50 %>= 50 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.030 %0.030 %
Chromium, Cr 17.5 %17.5 %
Iron, Fe 70.4 %70.4 %As Balance
Manganese, Mn 1.8 %1.8 %
Nickel, Ni 9.5 %9.5 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.60 %0.60 %
Sulfur, S <= 0.030 %<= 0.030 %
Titanium, Ti >= 0.15 %>= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV184 / 19078

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.