MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik SANMAC 4541 Billet
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: Sanmac 4541, is a titanium stabilized austenitic chrome-nickel steel with improved machinability.

Information provided by Sandvik

ASTM 321; UNS S32100; EN 1.4541

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 215
Tensile Strength, Ultimate 515 - 700 MPa
 >= 360 MPa
@Temperature 500 °C
 >= 375 MPa
@Temperature 300 °C
 >= 375 MPa
@Temperature 400 °C
 >= 390 MPa
@Temperature 200 °C
 >= 440 MPa
@Temperature 100 °C
Tensile Strength, Yield >= 210 MPa
@Strain 0.2 %
 >= 245 MPa
@Strain 1 %
 >= 119 MPa
@Strain 0.2 %,
Temperature 500 °C
 >= 125 MPa
@Strain 0.2 %,
Temperature 400 °C
 >= 135 MPa
@Strain 0.2 %,
Temperature 300 °C
 >= 149 MPa
@Strain 1 %,
Temperature 500 °C
 >= 155 MPa
@Strain 0.2 %,
Temperature 200 °C
 >= 156 MPa
@Strain 1 %,
Temperature 400 °C
 >= 167 MPa
@Strain 1 %,
Temperature 300 °C
 >= 175 MPa
@Strain 0.2 %,
Temperature 100 °C
 >= 185 MPa
@Strain 1 %,
Temperature 200 °C
 >= 205 MPa
@Strain 1 %,
Temperature 100 °C
Elongation at Break >= 40 %
Reduction of Area >= 50 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.030 %
Chromium, Cr 17.5 %
Iron, Fe 70.4 %As Balance
Manganese, Mn 1.8 %
Nickel, Ni 9.5 %
Phosphorus, P <= 0.040 %
Silicon, Si 0.60 %
Sulfur, S <= 0.030 %
Titanium, Ti >= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV184 / 19078

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.