MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

P & P Technology Aluminum 5056 (AMS 4182) Knitted Cored Shielding Mesh
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Product has a diameter of 0.11mm.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness  40 dB
@Frequency 10000 Hz
40 dB
@Frequency 10000 Hz
H-Field
 45 dB
@Frequency 100000 Hz
45 dB
@Frequency 100000 Hz
H-Field
 60 dB
@Frequency 1e+6 Hz
60 dB
@Frequency 1e+6 Hz
H-Field
 65 dB
@Frequency 1e+10 Hz
65 dB
@Frequency 1e+10 Hz
P-Field
 76 dB
@Frequency 1e+9 Hz
76 dB
@Frequency 1e+9 Hz
P-Field
 95 dB
@Frequency 4.00e+8 Hz
95 dB
@Frequency 4.00e+8 Hz
P-Field
 100 dB
@Frequency 1e+8 Hz
100 dB
@Frequency 1e+8 Hz
E-Field
 120 dB
@Frequency 1e+7 Hz
120 dB
@Frequency 1e+7 Hz
E-Field
 125 dB
@Frequency 1e+6 Hz
125 dB
@Frequency 1e+6 Hz
E-Field

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aleris HOGAL 5558 Aluminum 5026 H14/H34
Aleris Alustar H136 Aluminum Alloy
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy
Alcoa Deltalloy® 4032-T86 Aluminum
AISI E4340 Steel, heat treated, nitrided for 48 hrs., fatigue tested

PPPTEC012 / 133476

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.