MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Capron® 8202 NL Nylon 6 (Conditioned)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Information provided by BASF Corporation.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc(DAM); ISO 1183
Water Absorption 1.6 %24 hr. (DAM); ISO 62
 9.5 %(Beginning DAM); ISO 62
Moisture Absorption at Equilibrium 2.7 %23°C/50% R.H. (Beginning DAM); ISO 62
Viscosity Measurement 48Formic Acid; ASTM D789
Linear Mold Shrinkage 0.012 cm/cmMD; ASTM Test
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa0.2 in/min; ASTM D638
Tensile Strength, Ultimate 80.0 MPa
@Temperature -40.0 °C
ASTM D638
 80.0 MPa
@Temperature -40.0 °C
ISO 527
Tensile Strength, Yield 36.0 MPa50 mm/min; ISO 527
 36.0 MPa2 in/min; ASTM D638
 21.0 MPa
@Temperature 120 °C
ASTM D638
 21.0 MPa
@Temperature 120 °C
ISO 527
 30.0 MPa
@Temperature 80.0 °C
ASTM D638
 30.0 MPa
@Temperature 80.0 °C
ISO 527
 110 MPa
@Temperature -40.0 °C
ASTM D638
 110 MPa
@Temperature -40.0 °C
ISO 527
Elongation at Break >= 50 %50 mm/min; Nominal; ISO 527
 >= 100 %2 in/min; ASTM D638
 2.5 %
@Temperature -40.0 °C
ASTM D638
Elongation at Yield 16 %50 mm/min; ISO 527
 16 %2 in/min; ASTM D638
 35 %
@Temperature 80.0 °C
ASTM D638
 40 %
@Temperature 120 °C
ASTM D638
Tensile Modulus 0.970 GPa1 mm/min; ISO 527
Flexural Strength 35.0 MPaASTM D790
 155 MPa
@Temperature -40.0 °C
ASTM D790
Flexural Modulus 0.740 GPaASTM D790
 3.66 GPa
@Temperature -40.0 °C
ASTM D790
Izod Impact, Notched NBASTM D256
 0.450 J/cm
@Temperature -40.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10 K/min (DAM)
 220 °C(DAM); ASTM D3418
 
Compliance PropertiesOriginal ValueComments
FDA Yes21 CFR 177.1500
 
Descriptive Properties
AdditiveUnfilled
ColorNatural
Commercial Status (March 2007)Active America
FormPellets
Impact ModifiedNo
Injection moldingProcessable
Primary Processing TechniqueFilm Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Capron® 8200 NL Nylon 6 (Conditioned)
BASF Capron® 8202 NL Nylon 6 (DAM)
BASF Capron® 8202 HS BK-102 Nylon 6 (Dry)
BASF Ultramid® 8202 HS PA6 (Conditioned)
BASF Ultramid® 8202 PA6 (Dry)

PALBSE502 / 23153

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.