MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Capron® 8202 NL Nylon 6 (DAM)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Information provided by BASF Corporation.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Absorption 1.6 %1.6 %24 hr.; ISO 62
 9.5 %9.5 %ISO 62
Moisture Absorption at Equilibrium 2.7 %2.7 %23°C/50% R.H.; ISO 62
Viscosity Measurement 4848Formic Acid; ASTM D789
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inMD; ASTM Test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength at Break 75.0 MPa10900 psi0.2 in/min; ASTM D638
Tensile Strength, Yield 79.0 MPa11500 psi50 mm/min; ISO 527
 79.0 MPa11500 psi2 in/min; ASTM D638
 25.0 MPa
@Temperature 120 °C
3630 psi
@Temperature 248 °F
ASTM D638
 25.0 MPa
@Temperature 120 °C
3630 psi
@Temperature 248 °F
ISO 527
 35.0 MPa
@Temperature 80.0 °C
5080 psi
@Temperature 176 °F
ASTM D638
 35.0 MPa
@Temperature 80.0 °C
5080 psi
@Temperature 176 °F
ISO 527
 125 MPa
@Temperature -40.0 °C
18100 psi
@Temperature -40.0 °F
ASTM D638
 125 MPa
@Temperature -40.0 °C
18100 psi
@Temperature -40.0 °F
ISO 527
Elongation at Break 25 %25 %50 mm/min; Nominal; ISO 527
 55 %55 %2 in/min; ASTM D638
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527
 4.0 %4.0 %2 in/min; ASTM D638
 36 %
@Temperature 120 °C
36 %
@Temperature 248 °F
ASTM D638
 42 %
@Temperature 80.0 °C
42 %
@Temperature 176 °F
ASTM D638
Modulus of Elasticity  0.360 GPa
@Temperature 120 °C
52.2 ksi
@Temperature 248 °F
ISO 527
 0.485 GPa
@Temperature 80.0 °C
70.3 ksi
@Temperature 176 °F
ISO 527
Tensile Modulus 3.10 GPa450 ksi1 mm/min; ISO 527
Flexural Strength 110 MPa16000 psiASTM D790
 20.0 MPa
@Temperature 120 °C
2900 psi
@Temperature 248 °F
ASTM D790
 20.0 MPa
@Temperature 93.0 °C
2900 psi
@Temperature 199 °F
ASTM D790
 30.0 MPa
@Temperature 65.0 °C
4350 psi
@Temperature 149 °F
ASTM D790
 170 MPa
@Temperature -40.0 °C
24700 psi
@Temperature -40.0 °F
ASTM D790
Flexural Modulus 2.83 GPa410 ksiASTM D790
 0.305 GPa
@Temperature 120 °C
44.2 ksi
@Temperature 248 °F
ASTM D790
 0.350 GPa
@Temperature 93.0 °C
50.8 ksi
@Temperature 199 °F
ASTM D790
 0.500 GPa
@Temperature 65.0 °C
72.5 ksi
@Temperature 149 °F
ASTM D790
 3.01 GPa
@Temperature -40.0 °C
437 ksi
@Temperature -40.0 °F
ASTM D790
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inASTM D256
 0.500 J/cm
@Temperature -40.0 °C
0.937 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 83.0 µm/m-°C
@Temperature 20.0 °C
46.1 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 178 °C352 °FISO 75
 178 °C352 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75
 65.0 °C149 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1500
 
Descriptive Properties
AdditiveUnfilled
ColorNatural
Commercial Status (March 2007)Active America
FormPellets
Impact ModifiedNo
Injection moldingProcessable
Primary Processing TechniqueFilm Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® 8200 NL Nylon 6 (DAM)
BASF Capron® 8202 HS BK-102 Nylon 6 (Dry)
BASF Capron® 8202 NL Nylon 6 (Conditioned)
BASF Capron® B73MP Nylon 6 (DAM)
BASF Ultramid® 8202 HS PA6 (Conditioned)

PALBSE503 / 23154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.