MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPC 3150 MX5 Polypropylene, Heterophasic Copolymer, Automotive
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Polypropylene PPC 3150 MX5 is a high crystallinity and high impact polypropylene (HCPP) copolymer with a Melt Flow index of 15 g/10 min. The material is UV stabilized.

Polypropylene PPC 3150 MX5 is particularly suitable for the injection molding of automotive interior trims, door panels and instrument panels, using direct coloration with color masterbatches.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccISO 1183
Bulk Density 0.525 g/ccISO 1183
Linear Mold Shrinkage 0.014 - 0.016 cm/cm
@Thickness 3.00 mm
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ISO 868
Tensile Strength, Yield 29.0 MPaISO 527-2
Elongation at Yield 6.0 %ISO 527-2
Tensile Modulus 1500 MPaISO 527
 1740 MPaafter conditioning; ISO 527
Flexural Modulus 410 MPa
@Temperature 90.0 °C
ISO 178
 1400 MPa
@Temperature 23.0 °C
ISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²
@Temperature -20.0 °C
ISO 180
 9.00 kJ/m²
@Temperature 23.0 °C
ISO 180
Charpy Impact Unnotched NB
@Temperature -35.0 °C
ISO 179-1eU
Charpy Impact, Notched 3.20 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 5.00 kJ/m²
@Temperature -20.0 °C
ISO 179-1eA
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C120°C per hour; ISO 752
Vicat Softening Point 75.0 °C
@Load 5.10 kg
50°C per hour; ISO 306
 145 °C
@Load 1.02 kg
50°C per hour; ISO 306
 
Descriptive Properties
C-emission22 µgC/gVDA 277, VW 50180 - PV3015
Fogging0.4 mgDIN 75201-B, VW 50180 - PV3015
Odor3Scale 1 - 6, VDA 270, PV3200

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPC 3120 MU5 Polypropylene, Heterophasic Copolymer, Automotive
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact
Epsan Eplamid 66 GV0 25 NC Q1C5C001 Polyamide 66, Halogenated
Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive
Avient Trilliant™ HC FPO PPC-40T Natural PP Copolymer with 40% Talc

PTOTAL850 / 130575

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.