Flame retardant polyamide 66 reinforced with 25% of glass fiber, heat stabilized for injection molding. Halogenated flame retardant grade, compliance with RoHs derivatives, with rating UL94 V0 and glow-wire 960°C, combines excellent all around mechanical properties.Information provided by Epsan Plastik |