MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Solvay DAPCO™ 3004 Rapid Cure Epoxy Adhesive & Repair Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: DAPCO™ 3004 is a two-component, high strength, structural epoxy adhesive which cures at normal room temperature.

Features & Benefits:

  • Thixotropic flow properties permit use on vertical or overhead areas
  • Bonds a variety of substrates, including metal, wood, concrete and plastic
  • High resistance to cold and hot water, acids, alkalis, solvents, oils, grease, etc.
Applications: DAPCO 3004 is most commonly used as an insert potting compound as well as a general purpose adhesive. The product can be applied by extrusion, trowel, etc.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³Part A
 1.32 g/cc0.0477 lb/in³Mixed
 1.38 g/cc0.0499 lb/in³Part B
Solids Content 95 %95 %Part B
 98 %98 %Mixed
 100 %100 %Part A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85 - 9585 - 95
Tensile Strength 20.7 MPa3000 psi
Elongation at Break 3.0 %3.0 %
Adhesive Bond Strength 8.27 MPa1200 psiShear, Concrete/Concrete substrate failure
 11.0 MPa1600 psiShear, Stainless (321)
 11.7 MPa1700 psiShear, Aluminum (2024-T3)
 12.4 MPa1800 psiShear, Rigid PVC/PVC substrate failure
 13.8 MPa2000 psiShear, Plywood/plywood substrate failure
 16.5 MPa2400 psiShear, Carbon Steel
 
Descriptive Properties
ColorTanPart A
 TanPart B
 TanMixed
Mix Ratio1:1Volume
 100:107.5Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay DAPCO™ 3021C Low Viscosity, Self-Extinguishing Honeycomb Filler
ASTM A283 Steel, grade C
ASTM A139 Steel, grade C
Solvay DAPCO™ 3050 Epoxy Potting Compound
Solvay DAPCO™ 3012 Self-Extinguishing, Low Density Honeycomb Filler

PCYTED014 / 180316

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.