MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quantum Composites AMC™ 2593 45% Carbon Fiber Reinforced Phenolic SMC
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Composite SMC; Phenolic; Phenolic, Carbon Fiber Composite

Material Notes: AMC™ 2593 (126-40-139) is a carbon fiber reinforced phenolic engineered structural composite molding compound. The carbon fiber is PAN based 3K standard modulus tow. It exhibits outstanding low flow flammability characteristics. AMC™2593 (126-40-139) is recommended for applications such as aircraft interior and public transportation components requiring composite materials having very low flammability, low smoke, and minimal generation of toxic gases.

  • Form = Rolled Sheet
  • Color = Black or Natural
  • Carbon Fiber Content = Nominal - 45%

A. Schulman has acquired Quantum Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.55 g/ccASTM D792
Linear Mold Shrinkage 0.0015 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 258 MPaASTM D638
Tensile Modulus 62.0 GPaASTM D638
Flexural Strength 521 MPaASTM D790
Flexural Modulus 44.8 GPaASTM D790
Izod Impact, Notched 1281 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Smoke Density 2.0Ds; BSS7238
 
Processing PropertiesOriginal ValueComments
Shelf Life 2.00 Month
@Temperature 4.44 °C
 6.00 Month
@Temperature -17.8 °C
 
Descriptive Properties
Fiber Length (in)1Carbon, nominal
Flammability0 seconds, 1.4 inchesFAA Vertical Burn (60 sec)
 18 (2 min), 59 (peak)OSU Heat Release kW/m2, 0.080"
Toxicity of GassesPassBSS7239

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC
Solvay Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC

PCOQB910 / 139278

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.