MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Composite SMC; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: AMC™ 8595 is a vinyl ester engineered structural composite molding compound with continuous, unidirectional carbon fibers. It is designed for compression molding of components requiring high structural strength, light weight, and stiffness. It can also be co-molded with other ESC molding compounds such as AMC™ 8590 to provide stiffening in selected areas of the component.

  • Form = Rolled Sheet
  • Color = Natural, Black
  • Carbon Fiber Content = 55% nominal
  • Carbon Fiber Length = Continuous
  • Areal Weight = 1129 g/m2

A. Schulman has acquired Quantum Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D792
Water Absorption 0.11 %0.11 %ASTM D570
Linear Mold Shrinkage 0.00 cm/cm0.00 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 993 MPa144000 psiASTM D638
Tensile Modulus 94.5 GPa13700 ksiASTM D638
Flexural Strength 1310 MPa190000 psiASTM D790
Flexural Modulus 77.9 GPa11300 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 287 °C549 °FDeflection Temperature, Load not specified; ASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 132 - 149 °C
@Thickness 12.7 mm
270 - 300 °F
@Thickness 0.500 in
Compression Molding
Clamp Pressure 2.07 - 6.89 MPa300 - 1000 psi
Cure Time 3.00 - 5.00 min
@Thickness 6.35 mm,
Temperature 138 °C
0.0500 - 0.0833 hour
@Thickness 0.250 in,
Temperature 280 °F
Shelf Life 3.00 Month
@Temperature 23.9 °C
3.00 Month
@Temperature 75.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC
Solvay Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System

PCOQB909 / 139277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.