MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kazanorgsintez Butylene-Butadiene Fraction
Categories: Fluid

Material Notes: Production Method: Butylene-butadiene fraction is a by-product of ethylene production plants.

Application: BBF is used as feedstock for synthetic rubber production.

Information Provided by Kazanorgsintez

Key Words: BBF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Mass Content (%)0.5Mass content of C5+ Hydrocarbons, Grade D
 0.7Mass content of C3- Hydrocarbons, Grade D
 1.5Mass content of C3- and C5+ Hydrocarbons, Grade D
 15Mass content of C3- and C5+ Hydrocarbons, Grade D
 20Mass content of butadiene-1,3, Grades C and D
 30Mass content of butadiene-1,3, Grade B
 40Mass content of butadiene-1,3, Grade A
 5Mass content of C3- and C5+ Hydrocarbons, Grade D
 85Mass content of C4 Hydrocarbons, Grade D
 95Mass content of C4 Hydrocarbons, Grade C
 98Mass content of C4 Hydrocarbons, Grades A and B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Multibase Multi-Flex® G 7890 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Multibase Multi-Flex® G 7827 Black TPE Styrene Ethylene Butylene Styrene Block Copolymer
Multibase Multi-Flex® G 7715 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Multibase Multi-Flex® G 7705 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Multibase Multi-Flex® G 7680 TPE Styrene Ethylene Butylene Styrene Block Copolymer

PKAZAN187 / 127506

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.