MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase Multi-Flex® G 7827 Black TPE Styrene Ethylene Butylene Styrene Block Copolymer
Categories: Polymer; Thermoplastic

Material Notes:

Forms:

  • Pellets
  • Processing Methods:

  • Injection Molding
  • Uses:

  • Automotive Applications
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.16 g/cc1.16 g/ccASTM 792
    Melt Flow 60 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    60 g/10 min
    @Load 4.76 lb,
    Temperature 446 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 898910 seconds; ASTM D2240
    Tensile Strength, Yield 10.3 MPa1500 psiASTM D638
    Elongation at Break 550 %550 %ASTM D638
    Flexural Modulus 0.138 GPa20.0 ksiASTM D790
    Tear Strength 61.4 kN/m350 pliASTM D624
     
    Thermal PropertiesMetricEnglishComments
    Flame Spread 22.9 mm/min0.902 in/minFM VSS-302

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Overview of materials for High Density Polyethylene (HDPE), Injection Molded
    Overview of materials for Medium Density Polyethylene (MDPE), Molded
    Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
    Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer
    Multibase Multi-Flex® G 7155 TPE Styrene Ethylene Butylene Styrene Block Copolymer

    PMULTI088 / 53992

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.