MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Denka CL-430 Transparent Resin Polymer (MABS) ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a good balance of transparency, strength and fluidity (methyl methacrylate butadiene styrene), "TE Series/CL Series," transparent ABS resins with excellent color attributes and tensile strength are available (among others).

Applications

TX is used for:

  • flat display substrates
  • optical components
  • miscellaneous goods.
TP/TH are used for:
  • food package sheeting as well as in manufacturing
  • electronic equipment and components
  • miscellaneous goods
TE/CL are for:
  • electronic equipment and components
  • information equipment components
  • AV equipment, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Density 1.08 g/ccISO 1183
Melt Flow 2.7 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 34 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 31ISO 2039-2
Tensile Strength at Break 31.0 MPa50mm/min; ISO 527-2
 37.0 MPa50mm/min; ASTM D638
Elongation at Break 40 %50mm/min; ISO 527-2
Tensile Modulus 4.20 GPa50mm/min; ISO 527-1
Flexural Strength 62.0 MPaISO 178
 63.0 MPa2mm/min; ASTM D790
Flexural Modulus 2.00 GPa2mm/min; ISO 178
 2.01 GPa2mm/min; ASTM D790
Izod Impact Resistance 16.0 J/cm²
Charpy Impact, Notched 1.40 J/cm²ISO 179-2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °CISO 75-2
 72.0 °CASTM D648
Vicat Softening Point 80.0 °C50N; ISO 306
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %
@Thickness 2.00 mm
ISO 14782
Transmission, Visible 91 %
@Thickness 2.00 mm
ISO 13468-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Denka TE-30 Transparent Resin Polymer (MABS resin) ABS
INEOS Styrolution Terlux® HD 2802 MABS
INEOS Styrolution Terlux® 2802 Transparent MABS
Denka TE-10 Transparent Resin Polymer (MABS resin) ABS
Denka TE-20 Transparent Resin Polymer (MABS resin) ABS

PDENK019 / 29683

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.