MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Denka TE-30 Transparent Resin Polymer (MABS resin) ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a good balance of transparency, strength and fluidity (methyl methacrylate butadiene styrene), "TE Series/CL Series," transparent ABS resins with excellent color attributes and tensile strength are available (among others).

Applications

TX is used for:

  • flat display substrates
  • optical components
  • miscellaneous goods.
TP/TH are used for:
  • food package sheeting as well as in manufacturing
  • electronic equipment and components
  • miscellaneous goods
TE/CL are for:
  • electronic equipment and components
  • information equipment components
  • AV equipment, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Density 1.079 g/cc0.03898 lb/in³ISO 1183
Melt Flow  2.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.4 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 23 g/10 min
@Load 10.0 kg,
Temperature 220 °C
23 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 4242ISO 2039-2
Tensile Strength at Break 28.0 MPa4060 psi50mm/min; ISO 527-2
 32.0 MPa4640 psi50mm/min; ASTM D638
Elongation at Break 50 %50 %50mm/min; ISO 527-2
Tensile Modulus 3.90 GPa566 ksi50mm/min; ISO 527-1
Flexural Strength 60.0 MPa8700 psiISO 178
Flexural Modulus 1.80 GPa261 ksi2mm/min; ISO 178
Charpy Impact, Notched 1.90 J/cm²9.04 ft-lb/in²ISO 179-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C156 °FISO 75-2
 76.0 °C169 °FASTM D648
Vicat Softening Point 86.0 °C187 °F50N; ISO 306
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Haze 2.4 %
@Thickness 2.00 mm
2.4 %
@Thickness 0.0787 in
ISO 14782
Transmission, Visible 91 %
@Thickness 2.00 mm
91 %
@Thickness 0.0787 in
ISO 13468-1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Terlux® HD 2802 MABS
Denka CL-430 Transparent Resin Polymer (MABS) ABS
Denka TE-10 Transparent Resin Polymer (MABS resin) ABS
Denka TE-20 Transparent Resin Polymer (MABS resin) ABS
INEOS Styrolution Terlux® 2812 Transparent MABS

PDENK022 / 29686

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.