3M™ Dot Matrix Printable Polyimide Label Material 7811 is a polyimide film product that offers ultra-high temperature performance. This label product utilizes 3M™ Adhesive 100, that can withstand up to 450°F (232°C) short-term heat resistance, has excellent solvent resistance, and exhibits low outgassing characteristics.Information provided by 3M |