MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 7812 Thermal Transfer Polyimide Label Material
Categories: Polymer; Adhesive

Material Notes: 3M™ Thermal Transfer Polyimide Label Material 7812 is a polyimide film product that offers ultra-high temperature performance. This label product utilizes 3M™ Adhesive 100, that can withstand up to 450°F (232°C) short-term heat resistance, has excellent solvent resistance, and exhibits low outgassing characteristics

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 microns1.00 milFacestock, Matte White
 50.8 microns2.00 milFacestock, Polyimide Film
 50.8 microns2.00 milAdhesive
 81.3 microns3.20 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.351 kN/m2.00 pliStainless Steel, 180° Peel, 10 min Dwell at RT; ASTM D3330
 0.3725 kN/m2.125 pliPolycarbonate, 180° Peel, 10 min Dwell at RT; ASTM D3330
 0.482 kN/m2.75 pliEpoxy PC Board, 180° Peel, 10 min Dwell at RT; ASTM D3330
 0.482 kN/m2.75 pliEpoxy PC Board, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.58068 kN/m3.3125 pliStainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.614 kN/m3.50 pliPolycarbonate, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.6355 kN/m3.625 pliPolycarbonate, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.6793 kN/m3.875 pliEpoxy PC Board, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.6793 kN/m3.875 pliPolycarbonate, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.701 kN/m4.00 pliStainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.7231 kN/m4.125 pliStainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.73407 kN/m4.1875 pliEpoxy PC Board, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive Type100 Acrylic
Liner50# Densified Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film
CEN® Electronic Material CS Polyimide Tape
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler
3M 7811 Dot Matrix Printable Polyimide Label Material

PMM33413 / 168160

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.