MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LyondellBasell Petrothene® GA501023 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Applications
PETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent puncture resistance, elongation and heat seal strength. Applications include heavy duty shipping sacks, prime liners, commercial and industrial packaging, as well as food and consumer packaging.

Processing Techniques
Recommended conditions are 400-450°F melt temperature and a 1.5-3.01:1 blow-up ratio. Using proper techniques, this product can readily be drawn below 0.90 mil at optimum production rates. Specific recommendations for type of resin and extrusion conditions can be made only when the end use, required properties and processing equipment are known.

Regulatory Status
GA 501 series resins meet the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Thickness 38.1 microns1.50 mil2:1 BUR
Melt Flow 1.0 g/10 min1.0 g/10 min190/2.16; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 600 %600 %ASTM D882
Film Elongation at Break, TD 760 %760 %ASTM D882
Elmendorf Tear Strength MD 160 g160 gASTM D1922
Elmendorf Tear Strength TD 560 g560 gASTM D1922
Dart Drop Test 145 g0.320 lbF50; ASTM D1709A
Film Tensile Strength at Break, MD 40.0 MPa5800 psiASTM D882
Film Tensile Strength at Break, TD 31.7 MPa4600 psiASTM D882
1% Secant Modulus, MD 186 MPa27000 psiASTM D638
1% Secant Modulus, TD 241 MPa35000 psiASTM D638
 
Optical PropertiesMetricEnglishComments
Haze 11 %11 %ASTM D1003
Gloss 50 %50 %45°; ASTM D523
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
AntiblockMedium
SlipMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene
NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene

PEQU0336c / 36773

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.