MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Fireguard® 910L16-C1A-NL1 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Notes: RoHS Compliant

Features: Flame Retardant; Low Smoke Emission

Uses: Plenum Cable Jacketing

Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP

Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; UL 13; UL 1424; UL 1651; UL 444; UL QMTT2 .E200337

Processing Method: Extrusion

Forms: Pellets

Additional Notes:

Dynamic Heat Stability at 205°C, 100 rpm, 72 gr. #5 Bowl (Minutes to Decomposition): 34

Kayness ACR at 370°F, 1000 sec-1: 315 Pa-s

Kayness ACR at 370°F, 100 sec-1: 1243 Pa-s

Peak Heat Release Rate: 120 kW/m2

Average Heat Release Rate: 69 kW/m2

Total Heat Released: 65 MJ/m2

Average Heat of Combustion: 10.3 MJ/kg

Average Specification Extinction Area: 316 m2/kg

Peak Smoke: 1.91 1/m

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.62 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore C 8010 seconds; ASTM D2240
 89ASTM D2240
Tensile Strength at Break 2100 psiASTM D638
Elongation at Break 270 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.58
@Frequency 1e+6 Hz
ASTM D150
 4.56
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.038
@Frequency 1e+6 Hz
ASTM D150
 0.065
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 140 °FContinuous Use; ASTM D794
Brittleness Temperature -13.0 °FASTM D746
Oxygen Index 51 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 °F
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNO604 / 128782

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.