MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Fireguard® 910L16-C1A-NL1 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Notes: RoHS Compliant

Features: Flame Retardant; Low Smoke Emission

Uses: Plenum Cable Jacketing

Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP

Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; UL 13; UL 1424; UL 1651; UL 444; UL QMTT2 .E200337

Processing Method: Extrusion

Forms: Pellets

Additional Notes:

Dynamic Heat Stability at 205°C, 100 rpm, 72 gr. #5 Bowl (Minutes to Decomposition): 34

Kayness ACR at 370°F, 1000 sec-1: 315 Pa-s

Kayness ACR at 370°F, 100 sec-1: 1243 Pa-s

Peak Heat Release Rate: 120 kW/m2

Average Heat Release Rate: 69 kW/m2

Total Heat Released: 65 MJ/m2

Average Heat of Combustion: 10.3 MJ/kg

Average Specification Extinction Area: 316 m2/kg

Peak Smoke: 1.91 1/m

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.62 g/cc1.62 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore C 808010 seconds; ASTM D2240
 8989ASTM D2240
Tensile Strength at Break 14.5 MPa2100 psiASTM D638
Elongation at Break 270 %270 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.58
@Frequency 1e+6 Hz
3.58
@Frequency 1e+6 Hz
ASTM D150
 4.56
@Frequency 1000 Hz
4.56
@Frequency 1000 Hz
ASTM D150
Dissipation Factor  0.038
@Frequency 1e+6 Hz
0.038
@Frequency 1e+6 Hz
ASTM D150
 0.065
@Frequency 1000 Hz
0.065
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °FContinuous Use; ASTM D794
Brittleness Temperature -25.0 °C-13.0 °FASTM D746
Oxygen Index 51 %51 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 °C380 °F
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNO604 / 128782

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.