Chemical description: Silicone oil emulsion. Application fields GETREN® P 3000 is mainly used in dip coating of rubber seals to improve the sliding properties. Properties: - In the case that coated seals come into contact with acrylic glass, stress cracks will be avoided
- forms a hydrophobic protection coating
- improves the depth of color of the treated rubber
Information provided by Evonik |