MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Wacker® P Silicone Paste
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: WACKER® SILICONE PASTE P is a translucent, vaseline-like, relatively stiff, waterrepellent paste. WACKER® SILICONE PASTE P becomes softer when subjected to shear stress or other mechanical stress such as kneading, which in many instances makes processing easier. The pasty consistency is little affected by changes in temperature. The components of Paste P are on the positive lists of the following Regulations for food contact: Regulation (EU) No. 10/2011, Recommendation XV. Silicones of the BfR (Federal Institute for Risk Assessment) and the FDA Code of Federal Regulations Title 21 §175.3570 Lubricants with Incidental Food Contact.

Application: Assembly aid and lubricant for elastomers, especially O-rings. WACKER® SILICONE PASTE P is easy to apply. There is no dripping as when using oil. Larger parts are greased with the pure paste by hand or with abrush; smaller parts in large quantities are put into a plastic bag with some paste and kneaded until the paste has been distributed over their surfaces. Silicon pastes have only a slight swelling effect on most organic elastomers. For lubricating purposes and as assembly aid for materials with critical swelling characteristics we would, however, recommend using silicone product WACKER®POWERSIL® PASTE AP, which is especially designed for causing low swelling of bordering elastomers. Heat-resistance release agent for

  • extruder die rings
  • slightly porous surfaces of moulds for demoulding rubber and plastics mouldings and cast resin parts
  • heat-sealing instruments such as used for Packaging Film, where a thin film of WACKER® SILICONE PASTE P applied to the welding bars prevents sticking

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183-1 A
Volatiles <= 2.0 %
@Temperature 200 °C,
Time 108000 sec
<= 2.0 %
@Temperature 392 °F,
Time 30.0 hour
FED-STD 791 M 321
 
Mechanical PropertiesMetricEnglishComments
Penetration 180 - 220180 - 220[1/10 mm], unworked; DIN ISO 2137
Penetration P(60), 1/10 mm 250250worked; DIN ISO 2137
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.8
@Frequency 50 Hz
2.8
@Frequency 50 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inDIN 53481
Dissipation Factor 0.00050
@Frequency 50 Hz
0.00050
@Frequency 50 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Solidus -45.0 °C-49.0 °F
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
Appearancecolorless, opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Powersil® PASTE AP Silicone Paste
Mitsubishi Iupital® FS2022 Copolymer Acetal
ITW Devcon® Liquid Release Agent Silicone
Evonik TEGOPREN® 5863 Defoamer
Evonik TEGO® Antifoam 3062 Antifoam concentrate

PWACK9818 / 205347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.