MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Miracll H230 Thermoplastic Polyurethane Hot Melt/Solvent Adhesive
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Good solvent solubility, fast crystallization, excellent green bonding strength and final holding strength. Applications: fabric coating, fire hose adhesive, hot melt adhesive films & tapes, solvent adhesives, etc.

Information provided by Miracll Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Viscosity 2200 - 3600 cP15% in MEK, 25°C; ISO 3219
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ASTM D2240
Elongation at Break 600 %ASTM D412
Tear Strength 40.0 kN/mASTM D624
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 15.0 min
 
Descriptive Properties
Minimum Activation Temperature (°C)55-65
Tfb (°C)100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 3731 Hot Melt Adhesive
Miracll H320 Thermoplastic Polyurethane Hot Melt/Solvent Adhesive
Celanese Ateva® 2810A Ethylene Vinyl Acetate Copolymer
Chemical Concepts Chem-Set™ 707 High Performance Hot Melt
Braskem Evateno® HM 150 EVA Hot Melt Copolymer

PMIRAC70 / 221399

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.