MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemical Concepts Chem-Set™ 707 High Performance Hot Melt
Categories: Polymer; Adhesive; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: 707 is a high performance glue stick formulated specifically for bonding to difficult surfaces like metal, plastic, glass, ceramic and other porous and non porous materials. The 707 is a standard temperature hot melt that comes in a wide variety of glue stick sizes to match many different glue gun types.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 3125 cP
@Temperature 190.5 °C
3125 cP
@Temperature 374.9 °F
 
Thermal PropertiesMetricEnglishComments
Softening Point 81.1 °C178 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 191 °C375 °F
 
Descriptive Properties
Colorclear
Open Time30 seconds

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Ateva® 2810A Ethylene Vinyl Acetate Copolymer
Miracll H320 Thermoplastic Polyurethane Hot Melt/Solvent Adhesive
Miracll H230 Thermoplastic Polyurethane Hot Melt/Solvent Adhesive
Miracll H206 Thermoplastic Polyurethane Hot Melt/Solvent Adhesive
Michelman® Michem® Coat 40Y Water resistant, cold set and hot melt gluable coating

PCHEMI923 / 232215

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.