MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M 914 Repulpable Forms-Splicing Tape
Categories: Polymer; Tape

Material Notes: 3M™ Repulpable Forms-Splicing Tape 914 is a specially engineered forms-splicing tape using a thing, release-coated semi-bleached kraft paper backing and a blue, high performance repulpable adhesive. The construction is skip-slit fro easy separation.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 3.70 mil
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Break, MD 7.37 MPa
Film Tensile Strength at Break, TD 4.11 MPa
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
 
Descriptive Properties
Adhesive TypeBlue, repulpable
AppearanceOff-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 3320 HVAC Construction
Solvay RS 200 Sealant tape
Rogers Arlon R3781-920-##R##-P0 Silicone Rubber
Hexcel® HexPly® 914 175°C Curing Epoxy Matrix
Dymax 914-A Strain Relief, Wire and Parts Tacking Adhesive

PMM34525 / 169272

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.