MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dymax 914-A Strain Relief, Wire and Parts Tacking Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 914-A Strain Relief, Wire and Parts Tacking Adhesive
Faster curing, good insulation qualities, shock absorbing, deep cure capabilities and bonds well to porous surfaces Cure Type: UV

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 12000 cP12000 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 20.7 MPa3000 psi
 
Processing PropertiesMetricEnglishComments
Cure Time <= 0.0333 min<= 0.000556 hour
 
Descriptive Properties
Cure Depth0.375 in.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Dymax 9-911 Strain Relief, Wire and Parts Tacking Adhesive
Dymax 910 Strain Relief, Wire and Parts Tacking Adhesive
Dymax 9003v3.0 Flexible Clear Microencapsulant
Henkel Loctite® SpeedBonder™ 325 High Temperature Acrylic Bonding Adhesive

PDYYMAX34 / 35018

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.