MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBATER PBT A9030 gray 037091 (DB) PBT+PET, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: PBT+PET, 30% glass fiber reinforced grey, suitable for contact with food (EU)

Properties: dimensionally stable, good chemical resistance, good gliding properties, High strength, High stiffness, High wear resistance, semi-crystalline, approved for food contact (EU and FDA)

Typical areas of application: Cover, Electronic components, Housing, Crockery and cutlery, Food packaging, Connecting elements

Industries: Automotive, Electrical and electronics industry, Household appliances, Food processing industry, Mechanical Engineering, Sanitary industry

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³ISO 1183-1
Melt Flow 20.0 g/10 min
@Load 2.16 kg,
Temperature 270 °C
20.0 g/10 min
@Load 4.76 lb,
Temperature 518 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiISO 527-1
Elongation at Break 2.00 %2.00 %ISO 527-1
Modulus of Elasticity 8.50 GPa1230 ksiISO 527-1
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²ISO 179-1eU
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  HB
@Thickness 0.400 mm
HB
@Thickness 0.0157 in
IEC 60695-11-10
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 255 - 275 °C491 - 527 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 100 - 120 °C212 - 248 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.0200 %<= 0.0200 %
Back Pressure <= 4.00 MPa<= 580 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO689 / 326763

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.