MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik SOLIMIDE® HT 340 Polyamide Foam
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: SOLIMIDE HT-340 foam is typically utilized in commercial and industrial markets as a lightweight, fire resistant, thermal and acoustic insulation. It is also used in aerospace applications market where higher temperature resistance is needed. High temperature pipes and ducts, night storage heaters, and ovens are examples of applications that use SOLIMIDE HT-340 foam. A variety of shapes and sizes are available; facings or coatings are easily applied to suit end use requirements.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.00640 g/ccASTM D 3574
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 0.00483 MPa25% Deflection; ASTM D 3574
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0460 W/m-KASTM C 518
Maximum Service Temperature, Air 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik SOLIMIDE® Densified HT Foam
Evonik Solimide® HT-340 Polyimide Foam
Evonik SOLIMIDE® AC-530 Polyimide Foam
Evonik SOLIMIDE® AC-550 Polyimide Foam
DIAB Rigid Foam IPN 20-649 Type 1

PEVONIL905 / 197109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.