MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond F113 High Impact Optically Clear Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND F113 is an optically clear, low viscosity, high impact epoxy adhesive developed for bonding and small volume potting of plastic or glass optical fibers, lenses, and prisms, LED displays, and other optical components. It is recommended for laminating, bonding, and sealing applications where excellent wetting, good pot life and improved impact strength properties are required. This two part adhesive is easily mixed and cured at room temperature, and develops strong, tough bonds to glass and glass fibers, ceramics, many metals, and most rigid plastics. TRA-BOND F113 bonds offer resistance to mechanical impact and thermal shock, and are also resistant to weather, water, gases and vapors, petroleum products, salts, and mild acids and alkalis.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccMixed
Viscosity 180 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78
Adhesive Bond Strength 4000 psiLap shear, alum to alum, 2 hrs @ 65°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.00e+8 ohm-cm
Dielectric Constant 4.8
@Frequency 1000 Hz
Dielectric Strength 430 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 100 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 45.0 °CUltimate Tg
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.55
Transmission, Visible 97 %3200-9000 Å
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 120 min
Working Life 3.00 hour
 
Descriptive Properties
Color Transparent, Clear
Mix Ratio, parts by weight100/30Resin/Hardener
Thixotropic Index 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive
Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive
A. Schulman POLYBATCH™ Bright White LL80250 Concentrate Based In LLDPE
3M Dyneon™ Fluorel™ Dipolymer, 22% Carbon Black Filled
Avient PolyOne® 1601 Blue PEC Polyethylene

PTRAC225 / 71153

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.