MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. This room temperature curing system is an excellent choice for thin bond-line assembly and repair applications of prisms, lenses and other optic components. Its high strength makes this epoxy ideal for structural applications and its insulative properties are perfect for intricate bonding of electronic components. TRA-BOND F110 exhibits excellent wetting and wicking capabilities which allows it to adhere strongly to glass, ceramics, metals and most rigid plastics. Its highly structured matrix gives F110 good resistance to salt solutions, mild acids and alkalis and many other chemicals.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Volatile Organic Compounds (VOC) Content 39.1 g/l39.1 g/l
Viscosity 300 cP
@Temperature 25.0 °C
300 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Adhesive Bond Strength 14.8 MPa2150 psiLap shear, alum to alum, 24 hrs @ 25°C
 17.9 MPa2600 psiLap shear, alum to alum, 1 hr @ 65°C
 20.7 MPa3000 psiLap shear, alum to alum, 4 hrs @ 65°C
Izod Impact, Notched 0.128 J/cm0.240 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+13 ohm-cm6.00e+13 ohm-cm
Dielectric Constant 4.3
@Frequency 1000 Hz
4.3
@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm410 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C
@Temperature 20.0 °C
33.3 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 90.0 °C194 °FUltimate Tg
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54
Transmission, Visible 97 %97 %3200-9000 Å
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 65.0 °C
1.00 - 2.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 30 min30 min
Working Life 60.0 min60.0 min
 
Descriptive Properties
Color Transparent, Clear
Mix Ratio, parts by weight100/11Resin/Hardener
Thixotropic Index 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond F113 High Impact Optically Clear Epoxy Adhesive
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive
Avient PolyOne® 1601 Blue PEC Polyethylene
Avient PolyOne® 15077 White PEC Polyethylene
Avient PolyOne® 15020 White PEC Polyethylene

PTRAC223 / 71151

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.