With 4140 Chromoly steel, you can quickly reiterate and produce cost-effective tools and parts with complex geometries that are widely used in many applications of heavy industries such as automotive, oil and gas, agriculture or defense, printed Processed by DMSL on Studio System™, an office-friendly metal 3D printer. Having high torsional strength, 4140 can stand up to the stresses that couplings, for example, must withstand Processed by DMSL on a day-to-day basis. Applications: - Jigs and Fixtures
- Gears
- Automotive
- Couplings
- Bolts/Nuts
- Connecting Rods
Property data per MPIF Standard 35 Information provided by Proto3000 |
AISI 4140, UNS G41400, DIN 1.7200, JIS G4105 |