MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Proto3000 4140 Chromoly Steel MPIF 35-MIM Heat Treated
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Stainless Steel

Material Notes: With 4140 Chromoly steel, you can quickly reiterate and produce cost-effective tools and parts with complex geometries that are widely used in many applications of heavy industries such as automotive, oil and gas, agriculture or defense, printed Processed by DMSL on Studio Systemâ„¢, an office-friendly metal 3D printer. Having high torsional strength, 4140 can stand up to the stresses that couplings, for example, must withstand Processed by DMSL on a day-to-day basis.

Applications:

  • Jigs and Fixtures
  • Gears
  • Automotive
  • Couplings
  • Bolts/Nuts
  • Connecting Rods

Property data per MPIF Standard 35

Information provided by Proto3000

Key Words: AISI 4140, UNS G41400, DIN 1.7200, JIS G4105
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 7.50 g/cc
Porosity <= 4.50 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 46.0ASTM E18
Tensile Strength, Ultimate >= 1380 MPaASTM E8M
Tensile Strength, Yield >= 1070 MPaASTM E8M
Elongation at Break >= 3.00 %ASTM E8M
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.300 %
Chromium, Cr 0.800 - 1.20 %
Iron, Fe 96.6 - 99.0 %Balance
Manganese, Mn <= 1.00 %
Molybdenum, Mo 0.200 - 0.300 %
Silicon, Si <= 0.600 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NPROTO887 / 322900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.