MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Keysor-Century KYHH PVC Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); Polyvinyl Chloride - Polyvinyl Acetate Copolymer

Material Notes: A solution grade, medium molecular weight vinyl chloride-vinyl acetate copolymer resin. 18% Vinyl acetate. KYHH is soluble in esters, ketones, chlorinated hydrocarbons, and combinations of these with aromatic hydrocarbons to produce low solution rheological properties. White Free Flowing Powder

Recommended for printing ink and protective and maintenance coatings for masonry, metal, upholstery, paper, cardboard, foil, and marine applications.

Particle size: Nil retained on 32 mesh. 20% max through 200 mesh. Max volatiles 2%

Property values are typical values. Information provided by Keysor-Century Corporation.

Keysor-Century Corporation is no longer in business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccASTM D792
Apparent Bulk Density 0.690 g/ccASTM D1895
Brookfield Viscosity <= 300 cP
@Temperature 25.0 °C
25% resin solution in acetone, at 30 rpm
Viscosity Measurement 1.57Relative viscosity; ASTM D-1243

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Overview of materials for Polyvinyl Chloride - Polyvinyl Acetate Copolymer
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

PKCV06 / 48699

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.