MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro MAKROFOL® UV 503 9-2 060004 Polycarbonate Film
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC)

Material Notes: Makrofol UV 244 6-2 040004 is an coextruded film based on Makrolon® polycarbonate.

Properties / Applications: Makrofol UV 503 9-2 060004 comprises good light dispersion properties with all of the well known advantages of polycarbonate, such as excellent mechanical and optical properties. Typical application is automotive lighting. Makrofol UV 503 9-2 060004 is available in 0.010 ” to 0.030 ” (250 to 750 microns) standard thickness. Other thicknesses are available on request. The surface finish of Makrofol UV 503 9-2 060004 is velvet/very fine matte.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow <= 0.0040 cm/cm
@Time 3600 sec
<= 0.0040 in/in
@Time 1.00 hour
IEC 60674-2
Linear Mold Shrinkage, Transverse <= 0.0040 cm/cm
@Time 3600 sec
<= 0.0040 in/in
@Time 1.00 hour
IEC 60674-2
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 72.4 MPa10500 psiASTM D882
Tensile Strength, Yield 62.7 MPa9090 psiASTM D882
Elongation at Break 125 %125 %ASTM D882
Flexural Modulus 2.28 GPa331 ksiASTM D790
Tear Strength 210 kN/m1200 pliASTM D1004
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 - 120 °C
38.9 µin/in-°F
@Temperature 68.0 - 248 °F
DIN 53752
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 - 120 °C
38.9 µin/in-°F
@Temperature 68.0 - 248 °F
DIN 53752
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C264 °FASTM D648
Vicat Softening Point 143 °C289 °FRate A; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss <= 3.0 %<= 3.0 %60° top side black inked second surface; ASTM D2457
Transmission, Visible >= 85 %>= 85 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrofol® BL 2-4 820816 Polycarbonate
Covestro Makrofol® DE 1-1 000000 Polycarbonate
Covestro Makrofol® DE 7-2 Polycarbonate
Covestro Makrofol® DE 6-2 Polycarbonate
Covestro Makrofol® DE 1-4 000000 Polycarbonate

PCOVEST0816 / 202599

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.