MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrofol® DE 1-1 000000 Polycarbonate
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC)

Material Notes: Characterization: Makrofol DE 1-1 000000 is an extrusion film based on Makrolon® polycarbonate.

Properties / Applications: Makrofol DE 1-1 000000 comprises excellent transparence with high optical quality. Typical applications are automotive, labels, membrane switches, nameplates, and thermoform packaging. Makrofol DE 1-1 000000 is available in various standard thicknesses from 0.005 ” to 0.040 ” (125 microns to 1,000 microns). Other thicknesses are available on request. The surface combination of Makrofol DE 1-1 000000 is both sides gloss; one or both sides either with cling (C) or stick (S) masking. As with any product, use of Makrofol DE 1-1 000000 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.35 %
@Time 86400 sec
0.35 %
@Time 24.0 hour
immersion; ASTM D570
Water Absorption at Saturation 0.20 %0.20 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 72.4 MPa10500 psiASTM D882
Tensile Strength, Yield 62.7 MPa9100 psiASTM D882
Elongation at Break 125 %125 %ASTM D882
Flexural Modulus 2.28 GPa330 ksiASTM D790
Tear Strength 193 kN/m1100 pliASTM D1004
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 - 120 °C
38.9 µin/in-°F
@Temperature 68.0 - 248 °F
DIN 53752
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 - 120 °C
38.9 µin/in-°F
@Temperature 68.0 - 248 °F
DIN 53752
Flammability, UL94 V-2
@Thickness 0.381 mm
V-2
@Thickness 0.0150 in
Shrinkage  >= 0.40 %
@Temperature 130 °C,
Time 3600 sec
>= 0.40 %
@Temperature 266 °F,
Time 1.00 hour
parallel; IEC 60674-2
 >= 0.40 %
@Temperature 130 °C,
Time 3600 sec
>= 0.40 %
@Temperature 266 °F,
Time 1.00 hour
across; IEC 60674-2
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D1003
Gloss >= 90 %>= 90 %60° top side black inked second surface; ASTM D2457
 >= 90 %>= 90 %60° reverse side; ASTM D2457
Yellow Index 1.0 %1.0 %ASTM E313
Transmission, Visible 89 %89 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrofol® DE 1-4 000000 Polycarbonate
Covestro Makrofol® DE 6-2 Polycarbonate
Covestro Makrofol® BL 2-4 820816 Polycarbonate
Covestro Makrofol® DE 7-2 Polycarbonate
Covestro Makrofol® ID 4-4 Polycarbonate

PB09867 / 92707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.