MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M 8437 Two-Sided Metalized
Categories: Polymer; Tape

Material Notes: 3M™ Metalized Polyester Tape 8437 is comprised of relatively thin polyester backing with a metalized coating on both sides of the film providing a mirror-like finish with low emissivity and a versatile, long lasting acrylic adhesive. 3M tape 8437 is supplied on a silicone coated release liner for easy handling. The liner also allows for large area applications and die-cutting custom shapes. The liner also provides for additional stiffness and application ease when applying 3M tape 8437 in narrow gaps.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.900 milBacking; ASTM D3752
 2.10 milTotal; ASTM D3752
 4.30 milLiner; ASTM D3752
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaASTM D3759
Elongation at Break 70 %ASTM D3759
Peel Strength 2.50 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypeTransparent acrylic
AppearanceSilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Delrin® 100 AF Acetal Extruded Teflon® Filled Acetal
Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
DuPont Teijin Films Mylar® MDA Polyester Film, 48 Gauge
DuPont Mobility and Materials Vespel® SP-3 ISO Polyimide

PMM34491 / 169238

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.