MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow 111 VALVE LUBRICANT & SEALANT
Categories: Ceramic; Oxide; Silicon Oxide; Fluid; Lubricant; Silicone Base

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/cc
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Penetration 217Worked 100,000
Penetration P(60), 1/10 mm 205
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.17e+15 ohm-cm
Dielectric Constant 2.88
@Frequency 100 Hz
 2.95
@Frequency 100000 Hz
Dielectric Strength >= 450 V/mil
Dissipation Factor 0.00010
@Frequency 100 Hz
 <= 0.00050
@Frequency 100000 Hz
Arc Resistance 124 sec
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month
 
Descriptive Properties
Appearancetranslucent
Colorwhite
NLGI Number3
Water Resistantyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane
DuPont MOLYKOTE® 55 O-RING GREASE
Dow 41 High Temp. Bearing Grease
Phillips 66 Transformer Oil ISO Grade 10
Omni Plastics OmniTech™ PA6/6 SI2 FD Wear-and-Friction Silicone filled Nylon

PDOWCO245 / 105946

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.