MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow 41 High Temp. Bearing Grease  (discontinued **)
Categories: Fluid; Lubricant; Silicone Base

Material Notes: Former Dow Corning product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³
Saybolt Viscosity at 100°F 1740 SUS1740 SUSBase Oil Viscosity
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 240 kg529 lb (mass)
Four Ball Wear 3.00 mm0.118 inscar size
Penetration P(60), 1/10 mm 280280
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 288 °C550 °FContinuous
Minimum Service Temperature, Air -17.8 °C0.000 °F
 
Descriptive Properties
Bleed4.8%at 300°F
Dn Value75000
Drop Point>570°F
Evaporation2.5%at 300°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 111 VALVE LUBRICANT & SEALANT
Lord Adhesives Thermoset™ TC-330 Thermally Conductive Silicone Grease
Lord Adhesives Thermoset™ TC-208 Thermally Conductive Grease
Lord Adhesives Gelease™ MG-120 Thermally Conductive Silicone Gel Interface
ITW Permatex® Copper Anti-Seize Lubricant

PDOWC25 / 30741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.