MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Key Words: Polymer Technology & Services, LLC (PTS)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %24 hours at 73°F
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
6.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 62.1 MPa
@Thickness 3.17 mm
9010 psi
@Thickness 0.125 in
Elongation at Break 120 %
@Thickness 3.17 mm
120 %
@Thickness 0.125 in
Flexural Yield Strength 89.6 MPa
@Thickness 3.17 mm
13000 psi
@Thickness 0.125 in
Flexural Modulus 2.21 GPa
@Thickness 3.17 mm
321 ksi
@Thickness 0.125 in
Izod Impact, Notched 8.01 J/cm
@Thickness 3.17 mm
15.0 ft-lb/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FASTM D648
Flammability, UL94 V-2
@Thickness 1.59 mm
V-2
@Thickness 0.0625 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Clear grade, but transmission not quantified.
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 288 - 304 °C550 - 580 °F
Middle Barrel Temperature 299 - 321 °C570 - 610 °F
Front Barrel Temperature 316 - 338 °C600 - 640 °F
Nozzle Temperature 304 - 332 °C580 - 630 °F
Melt Temperature 316 - 343 °C600 - 650 °F
Mold Temperature 82.2 - 116 °C180 - 240 °F
Drying Temperature 121 °C250 °F
Dry Time 3 - 4 hour3 - 4 hour
Injection Pressure 110 - 138 MPa16000 - 20000 psi
Back Pressure 0.345 - 1.38 MPa50.0 - 200 psi
Clamp Pressure 27.6 - 68.9 MPa4000 - 10000 psi
Cycle Time - Injection 1.0 - 2.5 sec1.0 - 2.5 sec
Cycle Time - Cooling 5.0 - 40 sec5.0 - 40 sec
Vent Depth 0.00200 - 0.00800 cm0.000787 - 0.00315 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
Injection Speed- Edge GateSlow-Medium
Injection Speed- Tab GateMedium-Fast
Injection Speed- Tunnel GateFast
Shot Size40-60%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 603-3 Polycarbonate, Branched
Samyang Trirex® 3027U-C Polycarbonate, UV Stabilized
Lotte Advanced Materials Infino® SC-1060U PC Poly Optical Grade
LG Chemical Lupoy 1603-03 Polycarbonate Resin

PLBS23 / 50477

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.