MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Samyang Trirex® 3027U-C Polycarbonate, UV Stabilized  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electronic, appliance, automotive and optical industries.

UV-absorber concentrate

Applications:

  • Specially suitable for the production of coextruded UV screening layer on twin-wall or solid sheet

All information provided by Samyang

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 73.5 MPa10700 psiASTM D638
Elongation at Break 120 %120 %ASTM D638
Flexural Yield Strength 93.2 MPa13500 psiASTM D790
Flexural Modulus 2.16 GPa313 ksiASTM D790
Izod Impact, Unnotched 0.981 J/cm
@Thickness 3.17 mm
1.84 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C264 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 280 - 300 °C536 - 572 °F
Middle Barrel Temperature 280 - 300 °C536 - 572 °F
Front Barrel Temperature 280 - 300 °C536 - 572 °F
Nozzle Temperature 290 - 310 °C554 - 590 °F
Melt Temperature 300 - 310 °C572 - 590 °F
Drying Temperature 120 °C248 °F
Dry Time 3 - 5 hour3 - 5 hour
Moisture Content <= 0.020 %<= 0.020 %
Screw Speed 30 - 80 rpm30 - 80 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate

PSAMY069 / 88151

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.